30+ YEARS OF EXPERIENCE IN CARBON INDUSTRY

Knowledge
Home > Knowledge

Analysis of a New Electrode Hard Breakage Accident in a 25,000 kVA Ferro Silicon Electric

Time:2026-11-27   Traffic:1009
Arc Furnace

Electrode hard breakage accidents mainly occur during the charging process after electrode baking is completed. Such accidents generally occur at voltage levels 15–17, voltages of 160–175 V, electrode currents of 65–75 kA, and furnace power of 16–17.5 MW. The length of the hard breakage is generally 1.3–1.6 m, causing considerable trouble for furnace startup and making it very difficult to determine the tapping time of the first tap. If this is not determined accurately, it may result in the iron ladle being overfilled or difficulty in tapping the first tap.

ScreenShot_2026-11-27_161621_883.png

When electrode paste changes from solid to liquid, its mechanical strength reaches a minimum at 400°C. As the temperature rises from 400°C to 700°C, the mechanical strength increases sharply. Volatiles in the electrode paste begin to escape in large quantities at 400°C and are most intense at 500°C. When electrode baking enters the third stage at around 700°C, the remaining volatiles volatilize again. At 750°C, the electrode binder begins to carbonize. At 800°C, electrode baking is completed and the electrode reaches its final strength; thereafter, even if the temperature reaches 1,200°C, the electrode strength will not change significantly.

The above analysis shows that when the temperature is between 400°C and 700°C, the baking rate of the electrode determines the final quality of the electrode paste. If the sintering rate is too fast, volatiles are released intensely, which increases the porosity of the electrode itself and significantly reduces the quality of the baked electrode. This is one of the main factors causing electrode hard breakage accidents. Even if no hard breakage occurs, electrode pieces may still fall off during charging, causing the electrode consumption rate to be too high. In some cases, the working end of the electrode may become noticeably too short before the first tap, making tapping difficult. Even if the first tap is barely completed, the electrode must be baked immediately; otherwise, the furnace cannot be operated and tapping will be difficult. Conversely, if the baking rate is too slow, the furnace startup time is prolonged and the furnace cannot reach full efficiency as soon as possible, which is also undesirable.

PREVIOUS:Why does ash content affect electrode consumption?

NEXT:There is no more content!

Honesty connects the whole world
Rongxing adheres to the business philosophy of sincerity. From strategy formulation to raw material procurement, business negotiations, and technical services, we never cheat.
公司Logo
  • Rongxing Group focuses on product quality and reputation. It is a group company integrating the production and operation of electrode paste and graphite electrodes.
公司Logo
Products
Connect
  • PhonePhone:+86 19937179450
  • WhatsappWhatsapp:+86 19937179450
  • EmailEmail:[email protected]
  • AddressAdd:Zhengdong New District,Zhengzhou City,China.
Email
Message
Whatsapp
TOP